The fracture conduct and fracture manner on the diffusion-bonded joints were being elucidated by macro fracture and magnified surface area morphologies. The macro fracture morphologies (flat fracture) display that the propagation of crack happened along the MEA/DD5 interface in tensile checks in the joints achieved at 1020, 1050, and 1080 °C (Figu